3D printing Nickel-based superalloy IN738 powder

3D printing Nickel-based superalloy IN738 powder

3D printing Nickel-based superalloy IN738 powder

Detailed

3D printing Nickel-based superalloy IN738 powder

 

Composition(percentage by mass)

Ni

Cr

Co

Ti

Al

Mo

Ta

Bal

14.0-16.0

8.0-9.0

2.50-4.00

2.50-1-4.00

1.00-2.00

1.00-2.00

 


 

Ta

Nb

C

Fe

 Zr

B

O

1.00-2.00

0.50-1.50

<=0.15

<=0.10

<=0.10

<=0.15

<=0.01

 


 

category

Alloy grades and characteristics

Alloy number:

Nickel-based superalloy IN738 powder

Particle size:

15-45μm, 15-53μm, 53-120μm, 53-150μm

Morphology:

Spherical or nearly spherical

Appearance:

Grey

Package:

Aluminum bag,Vacuum packing

Application:

3D printing metal powder

Other applications:

powder metallurgy(PM), injection molding(MIM), spray painting(SP) etc.










 


                                                                                                                          








 